           was selected as presents less variation of viscosity with   Figures  10 and  11 show the variation  of storage
           the reaction time and a clear shear-thinning behavior   modulus (Gʹ), loss modulus (Gʺ), complex modulus, and
           being also less dependent with the reaction time compared   tan δ as a function of frequency and strain for systems
           to the other systems.                               containing 2% w/v alginate methacrylate concentrations

















                         a                                    b















                         c                                    d
           Figure 10. 2% wt. alginate solution reacted for 8 h. (a) storage and loss modulus versus strain (b) storage and loss modulus versus frequency,
           (c) complex modulus versus frequency, (d) tan δ versus frequency.














                         a                                    b
















                         c                                    d
           Figure 11. 2% wt. alginate solution reacted for 24 h. (a) storage and loss modulus versus strain, (b) storage and loss modulus versus
           frequency, (c) complex modulus versus frequency, (d) tan δ versus frequency.

                                       International Journal of Bioprinting (2019)–Volume 5, Issue 2        19