Page 130 - IJB-8-1
P. 130

Compression Failure of Trabecular Tantalum Scaffolds
                        A












                        B










           Figure 4. (A) Photographs and (B) optical micrographs of additive manufacturing-fabricated trabecular Ta scaffolds with porosities of 65%,
           75%, and 85%.

                        A











                        B




















           Figure 5. (A) Photographs and (B) scanning electron microscopy images of additive manufacturing AM-fabricated trabecular Ta scaffolds
           with porosities of 65%, 75%, and 85%.

           Table 1. Comparison of the porous characteristics of AM-fabricated trabecular Ta scaffolds with those of the designed models
           Models              Porosity (%)                Strut diameter (μm)          Average pore size (μm)
                         Design        Fabricated       Design        Fabricated       Design       Fabricated
           1               67           64.8±2.6         250          261.5±22.3        600         583.6±21.6
           2               77           75.3±1.7         250          259.2±25.5        800         779.8±34.2
           3               87           84.6±2.3         250          256.7±19.4        1000        986.3±45.4




           116                         International Journal of Bioprinting (2022)–Volume 8, Issue 1
   125   126   127   128   129   130   131   132   133   134   135