Materials Science in Additive Manufacturing                          Gradient porous material design criteria





                         A                                 B





























            Figure 2. (A and B) The 3D model and printed samples of the Schon-Gyroid and Schwarz-Diamond uniform porosity materials with the designs of 70 –
            71% (3/3), 70 – 72.5% (3/3), and 70 – 75% (3/3)



                         A                                 B



























            Figure 3. (A and B) The 3D model and printed samples of the Schon-Gyroid-sheet and Schwarz-Diamond-sheet uniform porosity materials with the designs of
            60 – 70 – 80% (2/2/2), 60 – 70 – 80% (3/2/1), and 70 – 80 – 90% (2/2/2)


            the first stress drop, the higher the possibility the sample   the stress exceeds the yield stress. As a result, it shows a
            will failure. On the other hand, if the toughness at the first   plateau deformation, where struts keep fracturing when the
            stress drop is significantly low, the crack will stop in the   stress exceeds the yield stress, thus causing displacement in
            porous material, and the other strut fracture occurs while   the second stage. Finally, in the third stage, the fractured


            Volume 3 Issue 3 (2024)                         4                              doi: 10.36922/msam.4234